b'Figure 3. Room-temperature tensile properties of hot-rolled and annealed C26M base alloys with various grain size.Figure 4. Surface cross-sectional views of C26M base alloys after steam ramp test up to 1450C.2019|AFC ACCOMPLISHMENTS 83'