2018 | AFC ACCOMPLISHMENTS 81 Figure 1: Comparison of historical wrought HT-9 to additive manufactured HT-9 in the as-built condition, FCRD heat treatment, and ACO3 heat treatment tensile properties including (a) yield strength - σʸ 0.2%, (b) ultimate tensile strength - σUTS, and (c) total elongation.